Description: AFM E309Mo-16 has the same composition of weld metal deposited by AFM E309-16,
except for the addition of molybdenum and a small reduction in the carbon
limit. It is used for welding Type 316 clad steels or for the overlay of carbon
steels.
Chemical Composition Requirements for Undiluted Weld Metal: |
(C) |
Carbon |
0.12 |
(Cr) |
Chromium |
22.0 to 25.0 |
| (Cu) |
Copper |
0.75 |
(Mn) |
Manganese |
0.5 to 2.5 |
(Mo) |
Molybtenum |
2.0 to 3.0 |
(Ni) |
Nickel |
12.0 to 14.0 |
(P) |
Phosphorus |
0.04 |
(S) |
Sulfer |
0.03 |
(Si) |
Silicon |
0.90 |
All values are considered maximum, unless other-wise noted.
All-Weld-Metal Mechanical Property Requirements (min.):
- Tensile Strength, psi 80,000
- MPa 550
- Elongation, (%)30
| Dia |
3/32 |
1/8 |
5/32 |
3/16 |
| MM |
2.4 |
3.2 |
4.0 |
4.8 |
Length |
12"
|
14" |
14" |
14" |
| Amps |
50-80 |
70-110 |
100-140 |
130-180 |
Packaging: All sizes are packaged in 10 lb. containers-3 containers per 30 lb. master carton.
|