AFM ER308L Stainless Steel Wire
AWS/SFA
A5.9
 
 

Description: This classification is the same as AFM ER308L, except for the higher silicon content. This improves the usability of the filler metal in the gas metal arc welding process. If the dilution by the base metal produces a low ferrite or fully austenitic weld, the crack sensitivity of the weld is somewhat higher than that of a lower silicon content weld metal.

Chemical Composition Requirements for Undiluted Weld Metal:

(C)

Carbon

0.03

(Cr) Chromium 19.5 to 22.0
(Cu) Copper 0.75
(Mn) Manganese 1.0 to 2.5
(Mo) Molybtenum 0.75
(Ni) Nickel 9.0 to 11.0

(P)

Phosphorus

0.03

(S)

Sulfer

0.03

(Si) Silicon 0.30 to 0.65
 

All values are considered maximum, unless other-wise noted.

 